2024/6/12
PE protective film preparation process

I. Key points of the process 1. Surface treatment of the base film Other additives, especially emulsifiers, will also have a significant impact on the performance of the adhesive for surface prote...

2024/6/11
Aluminium effect of aluminised film

Film surface treatment methods include corona treatment, plasma treatment, chemical treatment, photochemical treatment, flame treatment, and coating treatment. So which film surface treatment method i...

2024/6/5
Coating machine common problems and solutions

During the coating process, the phenomenon of poor coating gap and wrinkling of the pole piece is analysed: I. The phenomenon of poor coating gap and reasons 1. Tail dragging (1) material...

2024/6/3
Several common production lines for coating machines

Coating machine is mainly used for film, paper, etc. surface coating process production, this machine is the roll of substrate coated with a layer of specific function of the glue, paint or ink, etc...

2024/5/31
How to solve the irregular leakage in the coating process?

Causes. 1. The coating roller and bearing precision is not enough to form a regular crossbar path; 2. When the coating roller for the active drive, the choice of speed control programme is n...

2024/5/29
BOPP biaxially oriented film production line

BOPP biaxially oriented film production line produces products mainly used for books, periodicals, annual report cover, cardboard, gift bags, food packaging and other appearance of three-dimensional s...

2024/5/27
cpp vaporized barrier film production line

There are two major types of preparation methods for evaporated silicon oxide-based barrier packaging films: physical vapor deposition (PVC) and chemical vapor deposition (CVC). Depending on the speci...

2024/5/24
Analysis of the phenomenon of shrinkage and crimping of cast film

1¡¢ Shrinkage phenomenon The viscoelastic behavior of the polymer melt when the film is cast with a T-shaped die causes the following problems ¢Ù The width of the film narrows due to the shrinkage...